Cone 6 ≈ 2232 °F (1,222 °C) when the last part of the firing climbs at 108 °F (60 °C) per hour, and about 2269 °F (1,243 °C) at 270 °F (150 °C) per hour. Cone 5 is about 2167 °F and cone 7 about 2262 °F at the slower rate.
Mid-fire cones
| Cone | 108 °F/hr | 270 °F/hr |
|---|---|---|
| Cone 4 | 2124 °F / 1,162 °C | 2161 °F / 1,183 °C |
| Cone 5 | 2167 °F / 1,186 °C | 2205 °F / 1,207 °C |
| Cone 6 | 2232 °F / 1,222 °C | 2269 °F / 1,243 °C |
| Cone 7 | 2262 °F / 1,239 °C | 2295 °F / 1,257 °C |
A typical cone 6 glaze firing
Many studio schedules climb at about 200–300 °F per hour to around 2000 °F, then slow to about 100–150 °F per hour for the last 200 °F, with an optional short hold. Your kiln's preset cone 6 program and your glaze supplier's recommendations are the best starting point. Place witness cones on several shelves the first time you fire a new schedule.
See the full cone chart for every cone from 022 to 10.
Questions potters ask
Is cone 6 the same as 2232 °F?
Only at a final heating rate of 108 °F/hour. At 270 °F/hour cone 6 bends at about 2269 °F. Program your controller for the cone, or use witness cones to check.
What is the difference between cone 5 and cone 6?
About 65 °F at the same heating rate. Many cone 6 glazes are fine from cone 5 to 6; check how your glazes melt with witness cones.
Do I need a hold at cone 6?
Many potters use a short hold (often 10–15 minutes) or a slow-cool program to smooth glazes. Too long a hold adds heat work and can over-fire the glaze.
What clay fires at cone 6?
Mid-fire stoneware and porcelain bodies designed for cone 5–6. Low-fire earthenware will bloat or melt at cone 6.
How we estimate clay: the finished pot's wall and base volume × the fired density of the body, converted back to wet clay using typical water content and loss on ignition, plus a trimming and throwing allowance. Cone temperatures: Orton Ceramic Foundation published equivalents for self-supporting cones (°C converted). Glaze and plaster maths use standard slurry density relationships. Always follow your clay and glaze supplier's own data and safety sheets.